Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Styrolution® PS 7120 - (PS-HI) - INEOS Styrolution

Material Data Center offers the following functions for Styrolution® PS 7120:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other Styrolution PS datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Processing/Physical CharacteristicsValueUnitTest Standard
ASTM Data
Melt Flow Index, MFI 2.3 g/10min ASTM D 1238
Temperature 200 °C -
Load 5 kg -
Mold Shrinkage, MD 0.0055 mm/mm ASTM D 955
Mechanical propertiesValueUnitTest Standard
ASTM Data
Tensile Modulus 1793 MPa ASTM D 638
Tensile Strength at Yield 20.3 MPa ASTM D 638
Elongation at Break 55 % ASTM D 638
Flexural Modulus 1758 MPa ASTM D 790
Flexural Strength 44.1 MPa ASTM D 790
Rockwell Hardness L 42 - ASTM D 785
Izod Impact notched, 1/8 in 112 J/m ASTM D 256
Thermal propertiesValueUnitTest Standard
ASTM Data
UL 94 Flame rating HB - UL 94
Coefficient of Thermal Expansion, MD 90 E-6/K ASTM D 696
Vicat Temperature 103 °C ASTM D 1525
Electrical propertiesValueUnitTest Standard
ASTM Data
Dielectric Strength, Short Time 15.7 kV/mm ASTM D 149
Dielectric Constant, 1 MHz 2.5 - ASTM D 150
Optical propertiesValueUnitTest Standard
ASTM Data
Gloss 10 - ASTM D 2457
Other propertiesValueUnitTest Standard
Density 1040 kg/m³ ASTM D 792
Bulk Density 617 kg/m³ -
Characteristics
Special Characteristics
High impact or impact modified
Chemical Resistance
Environmental Stress Crack Resistance
Applications
Packaging, Refrigeration
Regional Availability
North America, South and Central America
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.